一.適用:
牛仔布(涂層布,壓光布除外)、硅油布、尼龍布、TPU、PU皮革等。
二.性能指標(biāo):
外觀及組成:白色狀粘稠體,聚氨酯聚合物
布氏粘度:120000~140000CPS
PH值:7.0±0.5
離子類型:陰離子
固體含量:50%±1
三.特性:
立體感強,高附著力,觸邊性好,透明性好,表面光滑。牢度超強、不粘手、高光澤、耐石磨洗、雪花洗、漂洗、酵素洗、酸洗、耐高溫蒸煮。耐黃變.5-35℃常溫下保存12個月,屬于環(huán)保型膠漿。
四.操作應(yīng)用:
1.本產(chǎn)品一般使用80目120目網(wǎng)布,根據(jù)圖案的不同絲網(wǎng)一定要繃緊,這一點相當(dāng)關(guān)鍵:
2.為了保證印制效果,一般不要制作太厚網(wǎng)版,根據(jù)厚度不同需要印5—8次,在使用厚網(wǎng)版印刷時印完第一次需待底層干透后再進(jìn)行第二次印刷,一般印刷3—4次就能達(dá)到2-3毫米以上的高度。
3.本產(chǎn)品不易塞網(wǎng),過稠時可加入適當(dāng)水漿攪拌均勻進(jìn)行稀釋。
4.在自然風(fēng)干48小時后,再過溫150度8-15秒,過溫時盡量將面料過反面。
5.如需提高牢度,使用時可加入1%-2%催化劑或交聯(lián)劑。
Otherdetailedinformation
Brand |
Conghui |
Model |
220 |
Viscosity |
/℃ |
PH |
℃ |
Odour |
/ |
Stretch |
100T |
fineness |
/um |
appearance |
|
Use |
|
Colorstrength |
100percent |
Fluidity≥ |
/mm |
expiration |
12months |
Singlenetweight |
5KG |
Resintype |
/ |
Ionperformance |
anion |
Surfacecolor |
|
一.Substrates
Uncoatedornon-presseddenim,siliconcoated,nylon,TPUorPUleather.
二.Indicatorsofperformance:
Appearanceandcomposition:whitedope,polyurethanepolymer
Brinellviscosity:120000~140000CPS
PH:7.0±0.5
Ionictype:anion
Solidcontent:50%±1
三.Productfeatures:
Highstackingproper,goodadhesionfastnesstofabrics,goodthixotropy,greattransparency,smoothfinish,superfastness,non-after tack,high glossiness,resistance to stone wash、snow wash、bleach、enzyme and acid wash.Resistance to high temperature steaming,yellowing.It can be stored at normal temperature of 5-35℃ for 12 months.It belongs to environmental paste.
四.Applicationofoperation
1.using80meshscreenand120meshscreen.Thekeypointisthescreenshouldbetightenedaccordingtodifferentpatterns.
2.Inordertoguaranteetheprintingeffect,donotmakethickaccordingtodifferentthicknessshouldbeprintedfivetoeighttimes.Whenusingthethickscreenprinting,youcanprintinthesecondtimeafterthebottomiscompletelydriedoffirsttime.Itcanreachmorethantwotothreemmheightwhenithasbeenprintedthreetofourtimesingeneral.
3.Thisproductiseasytoprintthroughfinemeshscreen,youcanaddappropriatewaterslurrytodilutewhentheitistoothick.
4.Afterthefortyeighthoursofnaturalairdry, and then over-temperature at 150℃ for 8-15 seconds.In the process of over-temperature,fabrics should be in opposite side as soon as possible.
5.Ifneedtoincreasethefastness,youcouldadd1-2% catalyst or cross-linker in usage.