一適用:
萊卡布,牛仔布(涂層布,壓光布除外)、尼龍布、TPU、PU皮革,及一些高彈性面料等.
二.性能指標(biāo):
外觀及組成:白色狀粘稠體,聚氨酯聚合物
布氏粘度:140000~160000CPS
PH值:7.0-8.0
離子類型:陰離子
固體含量:65%±1
三.特性:
立體感強(qiáng),觸邊性好,高附著力,高亮光,高彈性,手感超柔軟,抗回粘性能優(yōu)。表面光滑,牢度超強(qiáng)。耐高溫水洗、雪花洗、漂洗、酵素洗、酸洗、耐高溫蒸煮。(避免45℃以上高溫或—35℃以下低溫)優(yōu)越的低溫耐折。耐黃變.常溫下保存12個(gè)月,屬于高端環(huán)保型膠漿。本產(chǎn)品已通過(guò)國(guó)際一線品牌(耐克,卡帕,阿迪達(dá)斯)耐折,水洗反復(fù)測(cè)試。得到了權(quán)威的認(rèn)可。
PU0360立體水性墨白(機(jī)印超柔軟,似硅膠,雙組份):立體感強(qiáng),觸邊性好,高附著力,高亮光,拉伸力好,手感軟,柔軟似硅膠,干爽,耐高溫水洗,抗回粘性能優(yōu)。優(yōu)越的低溫耐折型,適合于機(jī)印
PU0360立體水性墨透(機(jī)印超柔軟,似硅膠,雙組份):立體感強(qiáng),觸邊性好,高附著力,高亮光,拉伸力好,手感軟,柔軟似硅膠,干爽,耐高溫水洗,抗回粘性能優(yōu),干擦4-5級(jí),濕擦4級(jí)。優(yōu)越的低溫耐折型,適合于機(jī)印
四.操作應(yīng)用:
1.本產(chǎn)品一般使用80目120目網(wǎng)布,根據(jù)圖案的不同絲網(wǎng)一定要繃緊,這一點(diǎn)相當(dāng)關(guān)鍵:
2.為了保證印制效果,一般不要制作太厚網(wǎng)版,根據(jù)厚度不同需要印5—8次,在使用厚網(wǎng)版印刷時(shí)印完第一次需待底層干透后再進(jìn)行第二次印刷,一般印刷3—5次就能達(dá)到2-3毫米以上的高度。
3.本產(chǎn)品不易塞網(wǎng),過(guò)稠時(shí)可加入適當(dāng)水漿攪拌均勻進(jìn)行稀釋。
4.在自然風(fēng)干48小時(shí)后,再過(guò)溫150度8-15秒,過(guò)溫時(shí)盡量將面料過(guò)反面。
5.使用時(shí)加入1%-2%交聯(lián)劑。(加好助劑的漿料要在3~6小時(shí)內(nèi)用完)
五、注意事項(xiàng):
1、自然干燥時(shí)間與氣溫和空氣濕度有關(guān)。
2、調(diào)色可根據(jù)客戶需要顏色的深淺來(lái)調(diào)入色種的分量,顏色調(diào)入太多容易引起掉色現(xiàn)象,色種最好控制在5%之內(nèi).
3、如印容易掉色的深色布,需要測(cè)試顏色是否會(huì)升華到膠漿表面上,以減少不必要的損失。
4、使用本透明產(chǎn)品印花,要稍加白膠漿摻和進(jìn)行調(diào)色印花有利于在紡織品面料上印花著色度飽和,更好發(fā)揮透明漿的應(yīng)用效果
5、由于印花面料的多樣化,和一些外在的不確定因素做大貨之前先小樣實(shí)驗(yàn)確定以后方可批量生產(chǎn)。未確定情況使用或操作不當(dāng)引起的質(zhì)量問(wèn)題本公司概不負(fù)責(zé).
Other detailed information
Brand |
Conghui |
Model |
0360 |
Viscosity |
/ |
PH Value |
7.0-8.0 |
Odor |
/ |
Strength |
100T |
Fineness |
/ |
Appearance |
/ |
Usage |
/ |
Color strength |
100% |
Fluidity |
/ |
Shelf life |
12months |
Single net weight |
20KG |
Resin type |
/ |
一.Substrates:
Lycra, denim(except coated fabric, press polishing fabric),nylon,TPU, PU leather and some high stretch fabric.
二.Performance indicators:
Appearance and composition: milky white viscous body, polyurethane polymer
Brinell viscosity:140000-160000CPS
PH Value:7.0-8.0
Ionic: anion
Solid content:65±1%
三.Features :
Super tomographic view, good side,high adhesion,glossiness and elasticity.super soft hand feel.Excellent anti after-tack,stain finish.Resistant to washing by high-temperature, snow wash,bleach,enzyme wash and acid wash. High temperature resistance steaming, yellowing resistance .The shelf life is 12months under normal temperature,belongs to high-end environmental paste.
PU0360 Stereo waterbased ink white(machine printing,super soft,just like silicone,two-component.):High three-dimensional sense,good edge,high adhesion,high glossiness,high tensile strength,soft hand feel,just like silicone,dry,resistance to high temperature washing,excellent performance of non-after tack.Excellent low temperature folding.By the way,it is suitable for machine printing.
PU0360 stereo waterbased ink clear(machine printing,super soft,just like silicone,two-component):High three-dimensional sense,good edge,high adhesion,high glossiness,good tensile strength,soft hand feel,just like silicone,dry,resistance to high temperature washing,excellent performance of non-after tack,the dry rub is 4-5 degree,the wet rub is 4 degree.Excellent low temperature folding.By the way,it is suitable for machine printing.
四.Operation application
1.This product usually use 80-120mesh screen, according to different patterns,the silk screen should be tightened, this one is very crucial.
2.In order to guarantee the printing effect,do not use too thick screen as usual,according to different thickness,print 5 or 8 times,when using thick screen to print,print in second time after the base dries completely in first time,as usual ,it can reach 2-3mm when printed 3-5times.
3.This product is not easy to mesh plug,when it is too thick, you could add appropriate water to stir evenly and mildly.
4.After air dry for 48 hours,and overheat at 150℃for 8-15seconds,when in the process of overheating should put the fabric in opposite side.
5.When using it,you could add 1%-2% catalyst or cross-linker.
五.Notes
1.The time of air dry is related to temperature and air humidity.
2.Adjusting color according to shade of color that customers need to add amount of pigment.If add too much it will lead to phenomenon of rubbing off, the amount of pigment should be controlled within 5%.
3.If prints on dark fabric that is easy to rub off, should be test color whether it sublimates on the surface of fabric,in order to reduce unnecessary financial losses.
4.Using clear product to print,should add white paste to adjust color printing,it makes printing looks full and reach the better application effect of clear paste.
5.Due to variety of fabric and some uncertain factors , you should make a test before in a batch production.Our company is not responsible for quality problem which caused by wrong operation or using under uncertain condition.